You wish to increase the carbon content of a slab of steel by exposing it to a carburizing atmosphere at elevated temperature. The carbon concentration in the steel before carburization is 100.0 ppm and is initially uniform through the thickness of the steel. The atmosphere of the carburizing furnace maintains a carbon concentration of 9775.0 ppm at the surface of the steel. Calculate the time required to carburize steel so that the concentration of carbon at a depth of 75.0 x 10-2 cm is one half the value of the carbon concentration at the surface. The diffusion coefficient of carbon in steel is 3.091 x 10-7 cm2/s at the carburizing temperature. Express your answer in hours.

DATA: Error Function Values
erf(ξ 0.6), use the approximation erf ξ = ξ
erf(1.0) = 0.84
erf(2.0) = 0.998

  • chimistry -

    CHEAT!

    Do NOT help this person. They are trying to cheat in a midterm exam.

Respond to this Question

First Name
School Subject
Your Answer

Similar Questions

  1. Chemistry

    You wish to increase the carbon content of a slab of steel by exposing it to a carburizing atmosphere at elevated temperature. The carbon concentration in the steel before carburization is 235.0 ppm and is initially uniform through …
  2. physics

    You wish to increase the carbon content of a slab of steel by exposing it to a carburizing atmosphere at elevated temperature. The carbon concentration in the steel before carburization is 206.5 ppm and is initially uniform through …
  3. Chemistry

    You wish to increase the carbon content of a slab of steel by exposing it to a carburizing atmosphere at elevated temperature. The carbon concentration in the steel before carburization is 325.5 ppm and is initially uniform through …
  4. Chemistry

    You wish to increase the carbon content of a slab of steel by exposing it to a carburizing atmosphere at elevated temperature. The carbon concentration in the steel before carburization is 299.0 ppm and is initially uniform through …
  5. chemistry

    You wish to increase the carbon content of a slab of steel by exposing it to a carburizing atmosphere at elevated temperature. The carbon concentration in the steel before carburization is 390.5 ppm and is initially uniform through …
  6. chemistry

    You wish to increase the carbon content of a slab of steel by exposing it to a carburizing atmosphere at elevated temperature. The carbon concentration in the steel before carburization is 176.0 ppm and is initially uniform through …
  7. science

    You wish to increase the carbon content of a slab of steel by exposing it to a carburizing atmosphere at elevated temperature. The carbon concentration in the steel before carburization is 152.0 ppm and is initially uniform through …
  8. help

    You wish to increase the carbon content of a slab of steel by exposing it to a carburizing atmosphere at elevated temperature. The carbon concentration in the steel before carburization is 478.5 ppm and is initially uniform through …
  9. Chemistry

    You wish to increase the carbon content of a slab of steel by exposing it to a carburizing atmosphere at elevated temperature. The carbon concentration in the steel before carburization is 359.5 ppm and is initially uniform through …
  10. chemistry

    You wish to increase the carbon content of a slab of steel by exposing it to a carburizing atmosphere at elevated temperature. The carbon concentration in the steel before carburization is 223.0 ppm and is initially uniform through …

More Similar Questions